Seyed Hossein Razavi, Mehdi Safavi, M. Reza Aboutalebi, Seyed Mehdi Abbasi,
Volume 21, Issue 0 (3-2024)
Abstract

This study examines how solution treatment temperature affects the dissolution of fine-grained areas (FGAs) that form during hot rolling of René 65 nickel-based superalloy. These FGAs, which are rich in sub-micron to micron-sized primary γ' precipitates (γ'I) and located mainly in shear bands, remained stable after sub-solvus treatments below 1055 °C. They dissolved gradually with increasing temperature and disappeared completely above 1115 °C. The resulting microstructural changes, along with high-temperature tensile properties and creep behavior in the 1055–1115 °C range (followed by aging at 760 °C for 8 h), were evaluated. Raising the solution temperature reduced the FGA volume fraction and improved tensile elongation, while yield strength (YS) and ultimate tensile strength (UTS) remained largely unchanged. At 1095 °C, creep life at 730 °C / 530 MPa exceeded 100 h without fracture and exhibited a notably lower steady-state creep rate. These improvements appear linked to the elimination of secondary γ' depleted zones around the former FGAs, which produced a more uniform secondary γ' distribution, greater crack path deflection, and continued Zener pinning by remaining primary precipitates. However, solution treatment at 1115 °C caused grain growth and coarsening of secondary precipitates, which reduced creep performance. Overall, 1095 °C provided the best compromise for microstructural uniformity and balanced high-temperature properties in hot-rolled René 65.

Page 1 from 1     

© 2022 All Rights Reserved | Iranian Journal of Materials Science and Engineering

Designed & Developed by : Yektaweb